联氨还原法制备镍纳米粒子

Preparation of nickel nanoparticles by reducing hydrazine

  • 摘要: 在表面活性剂聚乙烯吡咯烷酮(PVP)的保护下,采用水合肼于水体系中还原镍盐而得到镍纳米粒子。该粒子具有fcc相;表面价态为零价,说明制备过程中没有被氧化;粒子粒径在40 nm左右,近似圆球形,在正己烷中分散效果较好。

     

    Abstract: Nickel salts were reduced to nickel nanoparticles by hydrazine reduction method in the water system. The particles were packed by polyvinylpyrrolidone(PVP) to protect oxidation. The results of characterization show that the nickel nanoparticles consist of fcc phase, and the average size is about 40 nm. The circular grains are dispersed well in the hexane.

     

/