高压电常数PZT-PNN-PSN-PMW压电陶瓷的制备及性能研究
Microstructure and Enhanced Piezoelectric Properties of PZT-PNN-PSN-PMW Ceramic
-
摘要: 随着采用传统的固相反应制备了Pb0.92 Sr0.08(Zr0.48 Ti0.52)0.96-x(Ni1/3 Nb2/3)x(Sb1/3 Nb2/3)0.03(Mg1/ 2W1/2)0.01O3压电陶瓷(简称PZT-PNN-PSN-PMW)。通过XRD、SEM、阻抗分析仪等研究了PNN含量对陶瓷相结构、显微结构、介电性能和压电性能的影响。结果表明, 制备出了纯钙钛矿结构的PZT-PNN-PSN-PMW压电陶瓷, 随着PNN含量的减少, 其相结构由三方相向四方相转变。当x=0.2时, 在1280℃烧结的压电陶瓷具有最优的电学性能, 其压电常数d33、机电耦合系数kp、介电常数εr、居里温度Tc分别为电学性能为: 1035pC/N、83.4%、7895和122℃.Abstract: Pb0.92Sr0.08(Zr0.48Ti0.52)0.96-x(Ni1/3Nb2/3)x(Sb1/3Nb2/3)0.03(Mg1/2W1/2)0.01O3 piezoelectric ceramic (abbreviated as PZT-PNN-PSN-PMW) were synthesized by traditional solid-state reaction method.The effects of PNN content on phase structure, dielectric, piezoelectric properties of the ceramics were investigated in detail.The X-ray resulted that PZT-PNN-PSN-PMW ceramics are a pure perovskite structure without any other second phases, and their crystals structure transform from rhombohedral to tetragonal with decreasing PNN content.The piezoelectric ceramics with x=0.2 sintered at 1280℃exhibited the favorable electrical properties, which were listed as follows: d33=1035pC/N, kp=83.4%, εr=7895, Tc=122℃.
下载: